CORROSION PROTECTION




            It is the constant contact with salt water and salty atmospheres which requires the use of
            components with enhanced corrosion protection.
            The ranges of the materials used allow appropriate anti-corrosion protection of the
            external parts of the valve.





          K8: 500 -1000 H SALT SPRAY TEST
          All external elements on the valve which are in contact with   3  1       1
          the environment are surface-treated with a zinc-nickel coating
          or are made of stainless materials. Control knobs and partially
          knurled nuts are made of plastic.
          K8 will increasingly become the normal standard in the future.
          Only the valve flange bodies are painted and the screws zinc
          coated.


                                                               1                 5     1        1




          K9: > 1000 H SALT SPRAY TEST
          All external elements, apart from the solenoids, are made of   3  1       1
          stainless materials. Stainless, acid-resistant AISI 316L high-
          grade steels are used if feasable. The solenoids are zinc-nickel
          coated.







                                                               1                 4     2        2



          K10: > 1000 H SALT SPRAY TEST
          All extermal elements  are made of  stainless  materials  or   3  2       1
          coated with stainless materials. Stainless, acid-resistant AISI
          316L high-grade steels are used if feasable.








                                                               2                 4     2        2



                                                             Pos   Corrosion protection
                                                             1     Zinc-nickel coated
                                                             2     Stainless steel AISI 316L
                                                             3     Nickel coated brass
          * The salt spray test exposes the valve to a salt spray with a   4  Stainless steel screws
          five percent NaCl solution in accordance with ISO 9227. The   Zinc coated screws
          number of hours it takes for red rust to appear is measured.  5